Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.949 - 0.952 g/cc | 0.949 - 0.952 g/cc | ASTM D1505 |
LG Chemical SEETEC PM360 HDPE Features: Characteristics: Excellent processability, Good tenacity & knot strengthAdditives: Anti-oxidants, LubricantsApplication: Tarpaulin, Woven bags (Inflation)CAS No. 25213-02-9Information prov.. |
|||
Specific Gravity | 0.949 g/cc | 0.949 g/cc | ASTM D1505 |
SCG Chemicals EL-Leneâ„¢ H511W High Density Polyethylene Wire & Cable Grade Key Characteristics: Contains special metal deactivator, high mechanical properties, high speed extrusionRecommended Applications: Insulation of communication cablesInformation provided by SCG Che.. |
|||
Specific Gravity | 0.949 g/cc | 0.949 g/cc | ASTM D792 |
Total HDPE XT10 N High Density Polyethylene - Pipe Resin Polyethylene: High molecular weight, bimodal pipe resin.Characteristics:Outstanding high temperature creep rupture strengthExceptional slow crack growth resistanceExcellent resistance to rapid crac.. |
|||
Specific Gravity | 0.949 g/cc | 0.949 g/cc | ASTM D792 |
Total HDPE XT25N High Density Polyethylene, Pipe Resin Polyethylene: High molecular weight, bimodal pipe resin. PPI TR4 designation PE4710 /PE100 for demanding installations. Every batch certified to meet 2500 hrs PENT according to ASTM F1473.Charact.. |
|||
Specific Gravity | 0.949 g/cc | 0.949 g/cc | ASTM D1505 |
Chevron Phillips Marlex® 9509HF High Density Polyethylene, Blow Molding This gas phase, high molecular weight, hexane copolymer with synthetic antistatic agent is tailored for lightweight blow molded applications that:Require outstanding ESCRRequire excellent impact res.. |
|||
Specific Gravity | 0.949 g/cc @Temperature 25.0 °C |
0.949 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-200 20Cs Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 20CS. 100% active, 20 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Specific Gravity | 0.949 g/cc | 0.949 g/cc | ASTM D1505 |
Chevron Phillips Marlex® H516HP High Density Polyethylene, Pressure Pipe Grade This high performance PE 4710 HDPE is tailored for the demands of pressure pipe applications that require:Excellent long-term hoop strengthSuperb resistance to slow crack growthExceptional resistanc.. |
|||
Specific Gravity | 0.949 g/cc | 0.949 g/cc | ASTM D1505 |
Chevron Phillips Marlex® HP132 High Density Polyethylene, Pressure Pipe Grade This high performance PE 4710 HDPE is tailored for the demands of pressure pipe applications that require:Excellent long-term hoop strengthSuperb resistance to slow crack growthExceptional resistanc.. |