Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Braskem
Trade Name Green PE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SGF4960 is a homopolymer high-density polyethylene, developed for the blow-molding segment with high density and stiffness combined with high impact resistance. The minimum biobased content of this grade is 96%, determined according to ASTM D6866. Application: Bottles for food applications such as dairy products and beverages; Rigid containers for non-food applications such as cosmetics and lubricant oils; Caps & closures molded by compression; Rigid containers for pharmaceutical applications (complies with USP 33).Information provided by Braskem
Physical Properties Metric English Comments
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
ESCR 100% Igepal® 25 hour

@Temperature 50.0 °C
25 hour

@Temperature 122 °F
h/F50; Compression molded 2mm notched-plaques; ASTM D1693
Melt Flow 0.34 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.34 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
28 g/10 min

@Load 21.6 kg,
Temperature 190 °C
28 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength at Break 35.0 MPa
5080 psi
ASTM D638
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Izod Impact, Notched 2.25 J/cm
4.22 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C
174 °F
ASTM D648
Vicat Softening Point 129 °C
264 °F
10 N; ASTM D1525