Physical Properties Metric English Comments
Specific Gravity 1.70 - 1.80 g/cc
1.70 - 1.80 g/cc
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound
Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..
Specific Gravity 1.70 - 1.80 g/cc
1.70 - 1.80 g/cc
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound
Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..
Specific Gravity 1.30 - 1.80 g/cc
1.30 - 1.80 g/cc
ASTM D792
Parker Chomerics CHO-SEAL® 2557 Non-Conductive Extruded Elastomer Specifications
Description: Chomerics manufactures a dual performance extruded gasket in one simple design. By a seam vulcanization process, CHO-SEAL or CHO-SIL conductive elastomers are extruded in parallel with ..
Specific Gravity 1.70 - 1.80 g/cc
1.70 - 1.80 g/cc
ISO 1183
Raschig Group AMPLA® 2000 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve..
Specific Gravity 1.70 - 1.80 g/cc
1.70 - 1.80 g/cc
ISO 1183
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.78 - 1.80 g/cc
1.78 - 1.80 g/cc
ASTM D792
Arkema Group Kynar Flex® 2950 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound
A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Specific Gravity 1.60 - 1.80 g/cc
1.60 - 1.80 g/cc
IEC 1212-2 7.2
Hippe SI GC 41 Woven Glass Cloth Reinforced Silicone Resin - Round, Molded Tube and Rod
Used in mechanical, electrical and electronic applications. Good stability of electrical properties at elevated temperatures.Information provided by Hippe.
Specific Gravity 1.50 - 1.80 g/cc
1.50 - 1.80 g/cc
IEC 1212-2 7.2
Hippe EP MP 21 Mica Paper Reinforced Epoxy Resin - Round, Rolled Tube
Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity. Good heat resistance.Information provided by Hippe.
Specific Gravity 1.76 - 1.80 g/cc
1.76 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Specific Gravity 1.76 - 1.80 g/cc
1.76 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Specific Gravity 1.77 - 1.80 g/cc
1.77 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Gravity 1.77 - 1.80 g/cc
1.77 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Gravity 1.76 - 1.80 g/cc
1.76 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Specific Gravity 1.78 - 1.80 g/cc
1.78 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant
BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was..
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
Bulk Molding Compounds BMC 1412 Flame and Track Resistant
BMC 1412 is an extremely versatile material. Flame and track resistant, low shrink for close dimensional control and surface smoothness, high physical properties. Developed for injection molding, bu..
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)  (discontinued **)
Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.60 - 1.80 g/cc
1.60 - 1.80 g/cc
IEC 1212-2 8.1
Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet
Used in mechanical and electrical applications. High mechanical strength and good electrical properties under normal humidity. Heat resistant. Information provided by Hippe.
Specific Gravity 1.50 - 1.80 g/cc
1.50 - 1.80 g/cc
IEC 1212-2 7.2
Hippe PF GC 21 Woven Glass Cloth Reinforced Phenolic Resin - Round, Rolled Tube
Used in mechanical, electrical and electronic applications. Very high mechanical strength at moderate temperatures.Information provided by Hippe.
Specific Gravity 1.76 - 1.80 g/cc
1.76 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Specific Gravity 1.77 - 1.80 g/cc
1.77 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..