Physical Properties Metric English Comments
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
Noble Polymers Ecobarrier™ 2618 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
PolyOne Therma-Tech™ LC-5000C TC LCP  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
PolyOne Edgetek® SF-35GF-15MC/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
PolyOne Edgetek® SF-40GF-10 MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
SABIC Innovative Plastics Valox® 780 PBT
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific)
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine J-2 PVDF Extrusion Grade
Description: J-2 PVDF is a kind of granules homopolymer, which has middle melt viscosity, J-2 is more suitable for extrusion process. J-2 PVDF pellets as raw materials, the finished products has exc..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine M-1 PVDF Molding Grade
Description: M-1 PVDF is a kind of granules homopolymer, which has high melt viscosity, M-1 is more suitable for compression molding process. M-1 PVDF pellets as raw materials, the finished products..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine T-2 PVDF for Powder Coatings
Description: T-2 PVDF belong to thermoplastic fluorocarbon resin, which has high melt flow rate, low melt viscosity. T-2 PVDF has characteristic of chemical resistance, heat resistance, high mechani..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine Z-1 PVDF Injection Grade
Description: Z-1 PVDF is a kind of granular homopolymer, which has low melt viscosity, Z-1 is more suitable for injection molding. Z-1 PVDF pellets as raw materials, the finished products has excell..
Specific Gravity 1.77 g/cc
1.77 g/cc
Shinil Chemical SHINCON PES-CNT LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
E-Polymers TEKASTER® F615G55 55% Glass Fiber Reinforced High Modulus PET
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe..
Specific Gravity 1.77 g/cc
1.77 g/cc
BYK Cloisite® 20A Nanoclay
Cloisite® 20A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr..
Specific Gravity 1.77 - 1.80 g/cc
1.77 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Gravity 1.77 - 1.80 g/cc
1.77 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Gravity 1.77 - 1.80 g/cc
1.77 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Gravity 1.77 g/cc
1.77 g/cc
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine 904 PVDF for water UF (ultrafiltration) Membranes
Description: Ofluorine 904 PVDF Powder for water UF membranes has good solubility in some special solvent, which is a good raw material for PVDF UF membranes. Ofluorine 904 PVDF as raw materials, th..
Specific Gravity 1.77 - 1.80 g/cc
1.77 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Gravity 1.77 - 1.78 g/cc
1.77 - 1.78 g/cc
ISO R1183D
Shanghai Ofluorine 9201 PVDF Pellets for cables
Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, ..