Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00700 - 0.0150 cm/cm
0.00700 - 0.0150 in/in
Average value: 0.0130 cm/cm Grade Count:4
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported ..
Linear Mold Shrinkage, Transverse 0.00700 - 0.00800 cm/cm
0.00700 - 0.00800 in/in
Average value: 0.00780 cm/cm Grade Count:15
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Linear Mold Shrinkage, Transverse 0.00700 - 0.0120 cm/cm
0.00700 - 0.0120 in/in
Average value: 0.00995 cm/cm Grade Count:4
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a..
Linear Mold Shrinkage, Transverse 0.00700 - 0.0130 cm/cm
0.00700 - 0.0130 in/in
Average value: 0.00929 cm/cm Grade Count:14
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Linear Mold Shrinkage, Transverse 0.00700 - 0.0170 cm/cm
0.00700 - 0.0170 in/in
Average value: 0.0106 cm/cm Grade Count:22
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage, Transverse 0.00700 - 0.0120 cm/cm
0.00700 - 0.0120 in/in
Average value: 0.00888 cm/cm Grade Count:8
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Linear Mold Shrinkage, Transverse 0.00700 - 0.0150 cm/cm
0.00700 - 0.0150 in/in
Average value: 0.0108 cm/cm Grade Count:27
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Linear Mold Shrinkage, Transverse 0.00700 - 0.0243 cm/cm
0.00700 - 0.0243 in/in
Average value: 0.0164 cm/cm Grade Count:29
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..