Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.000800 - 0.105 cm/cm
0.000800 - 0.105 in/in
Average value: 0.00839 cm/cm Grade Count:221
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Linear Mold Shrinkage, Transverse 0.0000300 - 0.105 cm/cm
0.0000300 - 0.105 in/in
Average value: 0.00822 cm/cm Grade Count:114
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Linear Mold Shrinkage, Transverse 0.00530 - 0.105 cm/cm
0.00530 - 0.105 in/in
Average value: 0.00969 cm/cm Grade Count:54
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Linear Mold Shrinkage, Transverse 0.0075 - 0.105 cm/cm
0.0075 - 0.105 in/in
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Linear Mold Shrinkage, Transverse 0.0075 - 0.105 cm/cm
0.0075 - 0.105 in/in
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Linear Mold Shrinkage, Transverse 0.00450 - 0.105 cm/cm
0.00450 - 0.105 in/in
Average value: 0.00982 cm/cm Grade Count:19
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..