Polymer Property : Viscosity = 2.00e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1.00e+6 - 2.00e+6 cP

@Temperature 25.0 °C
1.00e+6 - 2.00e+6 cP

@Temperature 77.0 °F
Uncured
Permabond ES550 Epoxy Resin
PERMABOND ES550 is a single-part epoxy paste which is slump-resistant (does not flow) during cure. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear streng..
Viscosity 1.60e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.60e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Viscosity 1.50e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.50e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Viscosity 1.20e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.20e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR® 2821-00 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi..
Viscosity 1.20e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.20e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Viscosity 1.60e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.60e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..