Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.680 g/cc
0.0246 lb/in³
ASTM D4894
Solvay Specialty Polymers Algoflon® S 111 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
Apparent Bulk Density 0.680 g/cc
0.0246 lb/in³
ISO 60
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information..
Apparent Bulk Density 0.680 g/cc
0.0246 lb/in³
Ineos Barex® 218 E Acrylonitrile-Methyl Acrylate Copolymer
Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 218E is most commonly used for thermoformed sheet applications in which high impact performance is require..
Apparent Bulk Density 0.680 g/cc
0.0246 lb/in³
ASTM D1895
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided ..
Apparent Bulk Density 0.680 g/cc
0.0246 lb/in³
ASTM D1895
Sumitomo Bakelite Durez® 25378 Phenolic, Compression Grade
Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL ..
Apparent Bulk Density 0.680 g/cc
0.0246 lb/in³
ASTM D1895
Sumitomo Bakelite Durez® 25378 Phenolic, Injection Grade
Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL ..
Apparent Bulk Density 0.680 g/cc
0.0246 lb/in³
TRM-37
Tipco Tipcolite® THD 111 Phenolic Compound, Short Glass Fibers & Minerals, Medium -Soft Flow & High Strength
Medium -Soft Flow Phenolic Compound, Reinforced with Short Glass Fibres & MineralsApplications: Automotives & ElectricalProcessing: Compression & TransferInformation provided by the Manufacturer, T..
Apparent Bulk Density 0.680 - 0.800 g/cc
0.0246 - 0.0289 lb/in³
IS 867-1963
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded
Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg..
Apparent Bulk Density 0.680 - 0.720 g/cc
0.0246 - 0.0260 lb/in³
IS 867-1963
Amity Thermosets ATM 123 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownMedium flow..
Apparent Bulk Density 0.680 - 0.780 g/cc
0.0246 - 0.0282 lb/in³
IS 867-1963
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown..
Apparent Bulk Density 0.680 - 0.730 g/cc
0.0246 - 0.0264 lb/in³
IS 867-1963
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha..