Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.0 - 22 g/10 min | 5.0 - 22 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 7150 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 5.0 g/10 min | 5.0 g/10 min | ASTM D1238 |
Multibase Multi-Pro® 4005 M Polypropylene Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A; ASTM D1238 |
PolyOne Maxxam™ PPR-20G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers NPP 11-0535 Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc. |
|||
Melt Flow | 5.0 g/10 min @Load 1.00 kg, Temperature 235 °C |
5.0 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 2701T Transparent Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers Softflex® UB 30 Black OEX Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 5.0 - 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 - 12 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVALEN PC 51 T 30 Polypropylene Copolymer, 30% Micronized Talc FeaturesModified copolymer PP for injection moulding with the content of 30% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden f.. |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica.. |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 - 15 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical LUPOL HI5204H PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos R05C-00 Polypropylene Random Copolymer Random copolymer R05C-00 is an antistatic, clarified polypropylene random copolymer produced by a unique catalyst technology. It is designed as a high gloss resin and exhibits good stiffness and imp.. |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 7025 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 2.16 kg, Temperature 150 °C |
5.0 - 15 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-670 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 5.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass Information provided by Star Plastics, Inc. |
|||
Melt Flow | 5.0 - 15 g/10 min @Load 2.16 kg, Temperature 150 °C |
5.0 - 15 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-530 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SCG Chemicals EL-Leneâ„¢ LD1905FA Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex UNIPRENE® 2005 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 5.0 g/10 min | 5.0 g/10 min | ASTM D1238 |
A. Schulman PP 3482-01 Polypropylene Nucleated Homopolymer Polypropylene DescriptionPP 3482 is a nucleated homopolymer polypropylene with excellent heat resistance and stiffness properties.ApplicationThis product is for injection molded applications and is in compliance .. |
|||
Melt Flow | 5.0 g/10 min @Temperature 230 °C |
5.0 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Melt Flow | 5.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D 1238 |
Cossa Polimeri ESTASTIR HI 10 V0 Flame Retardant Polystyrene Flame retardant class V0, with PBDE, for injection molding or extrusionInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 5.0 g/10 min | 5.0 g/10 min | ASTM D1238-62T |
Chevron Phillips MarFlex® 4517 LDPE Extrusion Coating Resin Resin Type: HomopolymerCharacteristics: Excellent Processability, Good MVTR, Good Heat Seal, Kosher ApprovedApplications:Liquid Packaging, Cup Stock, Folding Carton, General CoatingData provided by .. |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ELASTO UK Dryflex® 660450S SEBS Based Material, Semi-Filled Qualities, 45A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 6301RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6301 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N.. |
|||
Melt Flow | 5.0 g/10 min | 5.0 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene HP0315V Homopolymer High Heat Approved to GMP.PP.013 |
|||
Melt Flow | 5.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Buckeye Polymers BP REPLEX 0805 R BLK ABS Polymer Product Information: Our BP REPLEX 0805 R BLK offers better than average impact while providing good melt flow characteristics in an affordably priced material.Product Features:Good impact and melt .. |
|||
Melt Flow | 5.0 - 10 g/10 min | 5.0 - 10 g/10 min | ASTM D1238 |
Aaron Industries AAROPRENE® GFABS 4040 Glass Filled Acrylonitrile-Butadiene Styrene AAROPRENE® GFABS 4000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Melt Flow | 5.0 g/10 min | 5.0 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Melt Flow | 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 50E631 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E631 is based on polypropylene homopolymer. They are available in pellet form for use in conventional extrusion and coextru.. |
|||
Melt Flow | 5.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
PlastxWorld CEVIAN®-V 320 ABS High Impact ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |