Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 40 g/10 min @Load 3.80 kg, Temperature 230 °C |
40 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 42 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® MT 10 Low Density Polyethylene - Injection Molding Riblene MT 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 are highly flexible.Main Applications: Riblene MT 10 is suitable for injection mo.. |
|||
Melt Flow | 40 - 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
40 - 45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 4341S Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 40 g/10 min @Load 8.40 kg, Temperature 360 °C |
40 g/10 min @Load 18.5 lb, Temperature 680 °F |
|
Performance Polymers IPS II PPL-A1050 PEKK (Polyetherketoneketone) Branched Standard Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Melt Flow | 40 g/10 min @Load 3.80 kg, Temperature 230 °C |
40 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 42 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 40 g/10 min @Load 0.325 kg, Temperature 270 °C |
40 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVASTER® B FRN 3 PBT, flame retarder FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® MT 10 R Low Density Polyethylene - Injection Molding Riblene MT 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 R are highly flexible.Main Applications: Riblene MT 10 R is suitable for inject.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips KN 230 LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware.. |
|||
Melt Flow | 40 - 90 g/10 min @Load 2.16 kg, Temperature 170 °C |
40 - 90 g/10 min @Load 4.76 lb, Temperature 338 °F |
DIN 53.735 |
Lubrizol Advanced Materials PEARLBOND® 108 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 108 is a linear, aromatic polycaprolactone-based polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a medium thermoplasti.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LM-4021-L LDPE Injection Molding Resin Features: Medium flow LDPE with a good balance of toughness, softness, dimensional stability and processability Applications: Injection molding of caps, closures and other specialty productsInformat.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 330 °C |
40 g/10 min @Load 4.76 lb, Temperature 626 °F |
|
Covestro Apec® DP 1-9339/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Melt Flow | 40 g/10 min @Load 10.0 kg, Temperature 380 °C |
40 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-7678 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Melt Flow | 40 g/10 min | 40 g/10 min | ASTM D1238 |
LyondellBasell Alathon® ETP H4837 High Density Polyethylene ApplicationsALATHON H 4837 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processability and thermal stability, with good color a.. |
|||
Melt Flow | 40 - 70 g/10 min | 40 - 70 g/10 min | Melt Volume Rate (cm³/10 min) |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 320 °C |
40 g/10 min @Load 11.0 lb, Temperature 608 °F |
ASTM D1238 |
LG Chemical LUCON PN9009 PPS+MF Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 230 °C |
40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go.. |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 250 °C |
40 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 250 °C |
40 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1551GN30 PBT, Impact Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1551GN30 is an impact grade.Information pro.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex TEKBOND® 6700-45 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 224 °C |
40 g/10 min @Load 11.0 lb, Temperature 435 °F |
ASTM D1238 |
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 230 °C |
40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 230 °C |
40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EM184AA Low Density Polyethylene WESTLAKE low-density polyethylene EM184 is a low density injection-molding formulation suggested for the production of closures where a high melt index is needed to meet shrinkage requirements and f.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding This hexene copolymer is tailored for injection molded applications that require:Excellent flowModerate impact strengthGood stiffnessTypical injection molded applications for 9035 include items such.. |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 190 °C |
40 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
ELASTO UK Mediprene™ 660440M TPE, Medical Applications, 44A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 275 °C |
40 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A34 01 PA66 (Conditioned) Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or .. |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 300 °C |
40 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
BLUESTAR LXS 112 PPE-PS Typical Applications: PV Industrial partsFire RatedInformation provided by Polymer Technology and Services, LLC (PTS). |