Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® HB6007 Blow Molding HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® HB6007 Blow Molding HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HomopolymerApplications: Milk, distilled water, soft drink concentrate, fruit juice, etc.Formolene HB6007 is a high quality product for those critical food packaging requirements. It also has excellent stiffness and good stiffness properties.Produced using licensor formulation for EHM 6007. Licensor does not warrant or imply that this product meets their specifications for EHM 6007.Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Nominal properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Physical properties are typical of product but do not reflect normal testing variance and therefore should not be used for specification purposes.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.964 g/cc
0.0348 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 10 hour
10 hour
Condition B, F<sub>50</sub>; ASTM D1693
15 - 20 hour
15 - 20 hour
Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693
Melt Flow 0.65 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.65 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.3 MPa
4400 psi
2" (50mm) per min.; ASTM D638 Type IV
Elongation at Break >= 300 %
>= 300 %
2" (50mm) per min.; ASTM D638 Type IV
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -118 °C
<= -180 °F
ASTM D746
Users viewing this material also viewed the following: