Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
12.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D123 |
Niche Polymer PCM12BK PC Information provided by Niche Polymer |
|||
Melt Flow | 12.0 - 25.0 g/10 min | 12.0 - 25.0 g/10 min | Average value: 16.4 g/10 min Grade Count:5 |
Overview of materials for PEN-PET This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1141 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 125 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 257 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1442A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 12.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
12.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1586UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2239 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2776A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2870M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1072 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Uses: Film; Sheet Forms: Pellets Processing Method: Injection Molding;.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® 90-E607D-88NT Ethylene Vinyl Acetate Copolymer Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4965A Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL EF-6155 UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1427A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2363A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2363B Thermoplastic Elastomer Availability: North America Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weath.. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2433A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2683B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 12.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
12.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Melt Flow | 12.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
12.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |
|||
Melt Flow | 12.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
12.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron TIM 200 MMA- ABS High Impact(Transparent ABS)Information provided by Bhansali |
|||
Melt Flow | 12.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
12.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Melt Flow | 12.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
12.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1537 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Melt Flow | 12.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
12.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Melt Flow | 12.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
12.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2870E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 12.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
12.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |