Physical Properties Metric English Comments
Melt Flow 12.0 - 25.0 g/10 min
12.0 - 25.0 g/10 min
Average value: 16.4 g/10 min Grade Count:5
Overview of materials for PEN-PET
This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent..
Melt Flow 6.27 - 25.0 g/10 min
6.27 - 25.0 g/10 min
Average value: 17.8 g/10 min Grade Count:13
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Melt Flow 0.600 - 25.0 g/10 min
0.600 - 25.0 g/10 min
Average value: 7.14 g/10 min Grade Count:42
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Melt Flow 3.00 - 25.0 g/10 min
3.00 - 25.0 g/10 min
Average value: 8.86 g/10 min Grade Count:38
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Melt Flow 3.00 - 25.0 g/10 min
3.00 - 25.0 g/10 min
Average value: 11.6 g/10 min Grade Count:9
Overview of materials for Polycarbonate, Foam Grade, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum ..
Melt Flow 10.0 - 25.0 g/10 min
10.0 - 25.0 g/10 min
Average value: 18.8 g/10 min Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
Melt Flow 10.0 - 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10.0 - 25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBW2442 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor..
Melt Flow 3.00 - 25.0 g/10 min
3.00 - 25.0 g/10 min
Average value: 10.3 g/10 min Grade Count:3
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Melt Flow 2.00 - 25.0 g/10 min
2.00 - 25.0 g/10 min
Average value: 13.4 g/10 min Grade Count:6
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Melt Flow 4.50 - 25.0 g/10 min
4.50 - 25.0 g/10 min
Average value: 10.6 g/10 min Grade Count:5
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Melt Flow 3.00 - 25.0 g/10 min
3.00 - 25.0 g/10 min
Average value: 9.65 g/10 min Grade Count:10
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Melt Flow 0.400 - 25.0 g/10 min
0.400 - 25.0 g/10 min
Average value: 6.85 g/10 min Grade Count:182
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..
Melt Flow 1.00 - 25.0 g/10 min
1.00 - 25.0 g/10 min
Average value: 5.63 g/10 min Grade Count:81
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..