Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12.0 - 25.0 g/10 min | 12.0 - 25.0 g/10 min | Average value: 16.4 g/10 min Grade Count:5 |
Overview of materials for PEN-PET This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent.. |
|||
Melt Flow | 6.27 - 25.0 g/10 min | 6.27 - 25.0 g/10 min | Average value: 17.8 g/10 min Grade Count:13 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Melt Flow | 0.600 - 25.0 g/10 min | 0.600 - 25.0 g/10 min | Average value: 7.14 g/10 min Grade Count:42 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Melt Flow | 3.00 - 25.0 g/10 min | 3.00 - 25.0 g/10 min | Average value: 8.86 g/10 min Grade Count:38 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Melt Flow | 3.00 - 25.0 g/10 min | 3.00 - 25.0 g/10 min | Average value: 11.6 g/10 min Grade Count:9 |
Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Melt Flow | 10.0 - 25.0 g/10 min | 10.0 - 25.0 g/10 min | Average value: 18.8 g/10 min Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Melt Flow | 10.0 - 25.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.0 - 25.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW2442 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 3.00 - 25.0 g/10 min | 3.00 - 25.0 g/10 min | Average value: 10.3 g/10 min Grade Count:3 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Melt Flow | 2.00 - 25.0 g/10 min | 2.00 - 25.0 g/10 min | Average value: 13.4 g/10 min Grade Count:6 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Melt Flow | 4.50 - 25.0 g/10 min | 4.50 - 25.0 g/10 min | Average value: 10.6 g/10 min Grade Count:5 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Melt Flow | 3.00 - 25.0 g/10 min | 3.00 - 25.0 g/10 min | Average value: 9.65 g/10 min Grade Count:10 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Melt Flow | 0.400 - 25.0 g/10 min | 0.400 - 25.0 g/10 min | Average value: 6.85 g/10 min Grade Count:182 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |
|||
Melt Flow | 1.00 - 25.0 g/10 min | 1.00 - 25.0 g/10 min | Average value: 5.63 g/10 min Grade Count:81 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |