Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Makroblend® DP 6015 Polycarbonate + PBT

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Covestro
Trade Name Makroblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Makroblend® DP 6015 Polycarbonate + PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade. Makroblend DP 6015* provides an outstanding balance of low-temperature impact strength and excellent chemical resistance having exceptional dimensional stability.PreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.02 g/cc

@Temperature 260 °C
0.0368 lb/in³

@Temperature 500 °F
Melt
Melt Flow 19 g/10 min

@Load 5.00 kg,
Temperature 260 °C
19 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
Nominal; ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
ISO 527-1/-2
Tensile Modulus 2.20 GPa
319 ksi
ISO 527-1/-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Specific Heat Capacity 1.82 J/g-°C
0.435 BTU/lb-°F
Melt
Thermal Conductivity 0.179 W/m-K
1.24 BTU-in/hr-ft²-°F
Melt
Deflection Temperature at 0.46 MPa (66 psi) 109 °C
228 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
260 °C
500 °F
Injection Molding; ISO 294
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
70.0 °C
158 °F
Injection Molding; ISO 10724
Ejection Temperature 170 °C
338 °F
Injection Velocity 200 mm/sec
7.87 in/sec
ISO 294
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
North America
South and Central America
Eff. thermal diffusivity (m²/s) 9.64E-08
Feature Release agent
Form Pellets
Process Injection Molding