Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 15 - 25 g/10 min @Load 11.6 kg, Temperature 250 °C |
15 - 25 g/10 min @Load 25.6 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Melt Flow | 12 - 25 g/10 min @Load 2.16 kg, Temperature 250 °C |
12 - 25 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Melt Flow | 10 - 25 g/10 min @Load 2.16 kg, Temperature 170 °C |
10 - 25 g/10 min @Load 4.76 lb, Temperature 338 °F |
DDIN 53.735 |
Lubrizol Advanced Materials Pearlbond® D170 Thermoplastic Polyurethane Pearlbond® D170 is a TPU grade designed for use with Heat Sealable Fabrics. This grade is to be applied in thermo bonding (heat-sealing) processes, through which the adhesive is laid on a series.. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 150 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-780 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized... |
|||
Melt Flow | 15 - 25 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 - 25 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Shanghai Ofluorine Z-1 PVDF Injection Grade Description: Z-1 PVDF is a kind of granular homopolymer, which has low melt viscosity, Z-1 is more suitable for injection molding. Z-1 PVDF pellets as raw materials, the finished products has excell.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 910 Utility Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 910-05V0 Utility Black Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 930 White Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 930-05V0 White Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 980 Grey Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman FR910V0 Utility Black Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman FR980V0 Grey Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman SP910 Utility Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.Data provided by the manufacturer. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman SP980 Grey Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.Data provided by the manufacturer. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 150 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-560 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 20 - 25 g/10 min @Temperature 230 °C |
20 - 25 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Melt Flow | 20 - 25 g/10 min @Temperature 230 °C |
20 - 25 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Melt Flow | 20 - 25 g/10 min @Temperature 230 °C |
20 - 25 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Melt Flow | 10 - 25 g/10 min @Load 8.70 kg, Temperature 210 °C |
10 - 25 g/10 min @Load 19.2 lb, Temperature 410 °F |
|
Lubrizol Estane® GP 58 DT Thermoplastic Polyurethane Type: Estane® GP 58DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |
|||
Melt Flow | 10 - 25 g/10 min @Load 8.70 kg, Temperature 210 °C |
10 - 25 g/10 min @Load 19.2 lb, Temperature 410 °F |
|
Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr.. |
|||
Melt Flow | 10 - 25 g/10 min @Load 8.70 kg, Temperature 170 °C |
10 - 25 g/10 min @Load 19.2 lb, Temperature 338 °F |
|
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Melt Flow | 10 - 25 g/10 min @Load 8.70 kg, Temperature 205 °C |
10 - 25 g/10 min @Load 19.2 lb, Temperature 401 °F |
|
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ISO 1133 |
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5.. |
|||
Melt Flow | 6.0 - 25 g/10 min @Load 12.5 kg, Temperature 232 °C |
6.0 - 25 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
Melt Flow | 6.0 - 25 g/10 min @Load 12.5 kg, Temperature 232 °C |
6.0 - 25 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 741 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 190 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 374 °F |
DIN 53.735 |
Lubrizol Advanced Materials PEARLBOND® 151 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 125/H is polycaprolactone-based thermoplastic polyurethane, supplied in form of colourless or slightly yellowish, translucid pellets, combining a low hardness with excellent low-temperat.. |
|||
Melt Flow | 8.0 - 25 g/10 min @Load 12.5 kg, Temperature 232 °C |
8.0 - 25 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2850 PC Polyvinylidene Fluoride Spray Coating Powder Electrostatic sprayInformation provided by Arkema Inc. |