Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shuman SP980 Grey Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Shuman
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shuman SP980 Grey Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Melt Flow 15 - 25 g/10 min
15 - 25 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Tensile Strength, Yield 66.0 MPa
9570 psi
ASTM D638
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
262 °F
ASTM D648
Vicat Softening Point 154 °C
309 °F
ASTM D1525
Flammability, UL94 V-2

@Thickness 1.57 mm
V-2

@Thickness 0.0618 in
Processing Properties Metric English Comments
Processing Temperature 266 - 287 °C
511 - 549 °F
Copyright © lookpolymers.com All Rights Reserved