Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 40 - 60 g/10 min @Load 5.00 kg, Temperature 250 °C |
40 - 60 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Melt Flow | 20 - 60 g/10 min | 20 - 60 g/10 min | 20-60 cm<sup>3</sup>/10 min; Melt Volume Rate |
Huntsman IROGRAN® A 78 P 4766 NM Ether-Based TPU-For Cable Industry TransparentInformation provided by Huntsman |
|||
Melt Flow | 30 - 60 g/10 min | 30 - 60 g/10 min | Melt Volume Rate (cm³/10 min) |
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Melt Flow | 30 - 60 g/10 min | 30 - 60 g/10 min | Melt Volume Rate (cm³/10 min) |
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Melt Flow | 30 - 60 g/10 min | 30 - 60 g/10 min | 30-60 cm<sup>3</sup>/10 min; Melt Volume Rate |
Huntsman IROGRAN® A 85 P 4666 Ether-Based TPU-For Cable Industry HFFR, radiation cross-linkableInformation provided by Huntsman |
|||
Melt Flow | 30 - 60 g/10 min @Load 2.16 kg, Temperature 170 °C |
30 - 60 g/10 min @Load 4.76 lb, Temperature 338 °F |
PMES11 |
Lubrizol Advanced Materials PEARLBOND® 121 Linear Thermoplastic Polyurethane Pearlbond™ 121 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Melt Flow | 40 - 60 g/10 min @Load 10.0 kg, Temperature 190 °C |
40 - 60 g/10 min @Load 22.0 lb, Temperature 374 °F |
ISO 1133 |
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane Pearlbond™ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus.. |
|||
Melt Flow | 30 - 60 g/10 min @Load 2.16 kg, Temperature 170 °C |
30 - 60 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials Pearlbond® ECO D590 Thermoplastic Polyurethane Pearlbond™ ECO D590 is a linear, aromatic bio-polyurethane based on specialty polyol from renewable sources, supplied in form of white spherical granules, with an extremely high crystallization.. |
|||
Melt Flow | 30 - 60 g/10 min @Load 2.16 kg, Temperature 170 °C |
30 - 60 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials Pearlbond® Eco D900 Thermoplastic Polyurethane Pearlbond™ ECO D900 is a linear, aromatic polyurethane based on specialty polyol from renewable sources. It contains 67% of renewable material as certified according to ASTM-D6866. It is suppli.. |
|||
Melt Flow | 50 - 60 g/10 min @Load 2.16 kg, Temperature 235 °C |
50 - 60 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melt Flow | 30 - 60 g/10 min @Load 2.16 kg, Temperature 170 °C |
30 - 60 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 101 Linear Thermoplastic Polyurethane Pearlbond™ 101 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve.. |
|||
Melt Flow | 30 - 60 g/10 min @Load 2.16 kg, Temperature 170 °C |
30 - 60 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 501 Linear Thermoplastic Polyurethane Pearlbond™ 501 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli.. |
|||
Melt Flow | 40 - 60 g/10 min @Load 2.16 kg, Temperature 150 °C |
40 - 60 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-706L TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hotmelt adhesiveHydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. U.. |
|||
Melt Flow | 55 - 60 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 - 60 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Polyram RamShine PV527 Acrylonitrile Butadiene Styrene, Flame Retardant Flame retardant ABS for injection molding applications.Information provided by Polyram. |
|||
Melt Flow | 30 - 60 g/10 min @Load 2.16 kg, Temperature 170 °C |
30 - 60 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 521 Linear Thermoplastic Polyurethane Pearlbond™ 521 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.Appl.. |