Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 9.00 - 12.0 microns | 0.354 - 0.472 mil | Fired |
Lord Adhesives Metech 3255 Silver Conductor This conductor composition is a silver bearing paste composition designed for screen print application of a solderable electrode base onto various types of electrical ceramic component devices. The .. |
|||
Thickness | 8.00 - 12.0 microns | 0.315 - 0.472 mil | cured |
Gwent Electronic Materials C2110127D3 Nanocopper based Paste This product is a nanocopper based paste for screen printing that is compatible with low temperature substrates such as paper. Produced using nanoparticles of negligible oxide content resulting in a.. |