Polymer Property : Thickness = 12.0 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 9.00 - 12.0 microns
0.354 - 0.472 mil
Fired
Lord Adhesives Metech 3255 Silver Conductor
This conductor composition is a silver bearing paste composition designed for screen print application of a solderable electrode base onto various types of electrical ceramic component devices. The ..
Thickness 8.00 - 12.0 microns
0.315 - 0.472 mil
cured
Gwent Electronic Materials C2110127D3 Nanocopper based Paste
This product is a nanocopper based paste for screen printing that is compatible with low temperature substrates such as paper. Produced using nanoparticles of negligible oxide content resulting in a..