Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 8.00 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 8.00 - 50.0 microns
0.315 - 1.97 mil
Recommended
Polimeri Europa Clearflex® CH D0 Very Low Density Polyethylene
Clearflex CH D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The film has a high stretchability and an optimum cling effect.Main Applications:..
Thickness 8.00 - 50.0 microns
0.315 - 1.97 mil
Recommended
Polimeri Europa Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene
Clearflex CL 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 106 are characterized by h..
Thickness 8.00 - 50.0 microns
0.315 - 1.97 mil
Recommended
Polimeri Europa Clearflex® CL 508 Octene Copolymer Linear Medium Density Polyethylene
Clearflex CL 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 508 exhibit a good bal..
Thickness 8.00 - 50.0 microns
0.315 - 1.97 mil
Recommended
Polimeri Europa Clearflex® CL D0 Very Low Density Polyethylene
Clearflex CL D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).This resin is produced with a proprietary technology. Stretch films manufactured..
Thickness 8.00 - 50.0 microns
0.315 - 1.97 mil
Recommended
Polimeri Europa Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T CLH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CLH 108 show e..
Thickness 8.00 - 50.0 microns
0.315 - 1.97 mil
Recommended
Polimeri Europa Clearflex® H&T CLH 150 Linear Low Density Polyethylene
Clearflex H&T CLH 150 is a linear low density polyethylene resin, with antioxidants, suitable for cast film extrusion.Stretch films obtained from Clearflex H&T CLH 150 show good optical properties, ..
Thickness 8.00 - 50.0 microns
0.315 - 1.97 mil
Recommended
Polimeri Europa Clearflex® CL B0 Very Low Density Polyethylene
Clearflex CL B0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has a high stretchability and a good cling effect.Main Applications: C..
Thickness 8.00 - 50.0 microns
0.315 - 1.97 mil
Recommended
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene
Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h..
Thickness 8.00 - 50.0 microns
0.315 - 1.97 mil
Recommended
Polimeri Europa Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T CMH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CMH 108 show e..
Thickness 8.00 - 12.0 microns
0.315 - 0.472 mil
cured
Gwent Electronic Materials C2110127D3 Nanocopper based Paste
This product is a nanocopper based paste for screen printing that is compatible with low temperature substrates such as paper. Produced using nanoparticles of negligible oxide content resulting in a..
Thickness 8.00 - 51.0 microns
0.315 - 2.01 mil
Average value: 29.6 microns Grade Count:16
Overview of materials for Very Low Density Polyethylene (VLDPE)
This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va..
Thickness 8.00 - 76.2 microns
0.315 - 3.00 mil
Average value: 31.0 microns Grade Count:152
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..
Thickness 8.00 - 50.0 microns
0.315 - 1.97 mil
Average value: 29.0 microns Grade Count:64
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m..
Thickness 8.00 - 150 microns
0.315 - 5.91 mil
Average value: 33.9 microns Grade Count:20
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum..
Thickness 8.00 - 75.0 microns
0.315 - 2.95 mil
Average value: 31.5 microns Grade Count:8
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and..
Thickness 8.00 - 50.0 microns
0.315 - 1.97 mil
Recommended
Polimeri Europa Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene
Clearflex H&T CLH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Stretch films manufactured with Clearflex H&T CLH 196 have..
Copyright © lookpolymers.com All Rights Reserved