3M 7037 Screen Printable Polyester Performance Label Product

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7037 Screen Printable Polyester Performance Label Product.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Screen Printable Polyester Performance Abel Product 7037 is a durable, high performance material that offers excellent thermal stability and moisture resistance. This polyester label stock utilizes 3M™ Adhesive 350, which is designed to permanently bond to high and low surface energy plastics, textured and contoured surfaces, powder coatings, and slightly oily metal.Information provided by 3M
Physical Properties Metric English Comments
Thickness 27.9 microns
1.10 mil
Facestock
178 microns
7.00 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.351 kN/m
2.00 pli
0.614 kN/m
3.50 pli
0.614 kN/m
3.50 pli
0.789 kN/m
4.50 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Application
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Application
50.0 °C
122 °F
Service
Descriptive Properties Value Comments
Adhesive Type 350
Liner 90# Polyctd.