Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.55 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.55 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene BM3245 PC High Density Polyethylene CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS:PIPE EXTRUSIONSUI.. |
|||
Melt Flow | 0.55 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.55 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® BB 10 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB 10 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.55 g/10 min @Load 2.16 kg |
0.55 g/10 min @Load 4.76 lb |
ISO 1133 |
Total 8183 HDPE, blow molding Applications: cosmetic bottles, pharmaceutical bottles, industrial product containers, chemical packaging, food packagingInformation provided provided by Total Petrochemicals.Total Petrochemicals ac.. |
|||
Melt Flow | 0.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total HDPE 7194 High Density Polyethylene, Specialty Extrusion Resin Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationUSP Class VI compliantApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformat.. |
|||
Melt Flow | 0.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total HDPE 7195 High Density Polyethylene, Specialty Extrusion Resin Characteristics:Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformation pr.. |
|||
Melt Flow | 0.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem GM5340PR High Density Polyethylene Triple-layer coating for metallic pipes; Umbilical pipes for offshore oil field platforms; Jacketing for wires and for optic fiber metallic cables; Self-propelled irrigation pipes; Localized irrigat.. |