Braskem GM5340PR High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem GM5340PR High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Triple-layer coating for metallic pipes; Umbilical pipes for offshore oil field platforms; Jacketing for wires and for optic fiber metallic cables; Self-propelled irrigation pipes; Localized irrigation pipes; Ducts for mining.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.959 g/cc
0.959 g/cc
ASTM D1505/D792
ESCR 100% Igepal® >= 1000 hour

@Temperature 50.0 °C
>= 1000 hour

@Temperature 122 °F
h/50%f; compression molded 2 mm notched-plaques; ASTM D1683
ESCR 10% Igepal® 200 hour

@Temperature 50.0 °C
200 hour

@Temperature 122 °F
h/50%f; compression molded 2 mm notched-plaques; ASTM D1683
Melt Flow 0.55 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.55 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
39 g/10 min

@Load 21.6 kg,
Temperature 190 °C
39 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Flexural Modulus, 1% Secant 980 MPa
142000 psi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C
154 °F
ASTM D648
Vicat Softening Point 121 °C
250 °F
ASTM D1525