Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 1.3 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 1.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Ravago Manufacturing Americas Hylac® GP48 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Melt Flow 1.3 - 1.9 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.3 - 1.9 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE
Namtene® 1002 is used for pipes. It features a lower polypropylene content than standard Namtene®.
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis BB125MO Polypropylene Copolymer
BB125MO is a heterophasic copolymer. This grade is a low melt flow rate grade intended for blow molding and sheet extrusion, and features extremely good process ability with improved melt strength a..
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection
BB412E is a natural, medium molecular weight, medium melt flow rate polypropylene block copolymer with an optimal mechanical properties balance resulting in high stiffness and very good impact stren..
Melt Flow 1.3 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Borealis BS2581 High Density Polyethylene for Blow Molding
BS2581 is a high density polyethylene intended for blow molding products with high stiffness and very good environmental stress crack resistance (ESCR). Applications: industrial chemicals, househol..
Melt Flow 1.3 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Unipetrol PE HD LITEN® VB 33 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Melt Flow 1.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 4000HH
Description: Heat Resistant Grade, Medium High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 1.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 4000HH-ELG
Description: Heat Resistant Grade, Low Gloss, Medium High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 1.3 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.3 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA 5946
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 1.3 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.3 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA S519
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 1.3 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.3 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA TW-18B2
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 1.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers SAN 250 with Lube Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 1.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ASA TWP 502
Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc.
Melt Flow 1.3 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications
Bormed HE2581-PH is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR). Bormed HE2581-PH can as well be ..