Unipetrol PE HD LITEN® VB 33 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Unipetrol RPA
Trade Name PE HD LITEN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unipetrol PE HD LITEN® VB 33 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ISO 1183
ESCR 100% Igepal® 11 hour

@Temperature 50.0 °C
11 hour

@Temperature 122 °F
ASTM D1693
Melt Flow 0.33 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.33 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
1.3 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.3 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
21 g/10 min

@Load 21.6 kg,
Temperature 190 °C
21 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ISO 868
Tensile Strength, Yield 27.0 MPa
3920 psi
ISO 527
Elongation at Yield 9.0 %
9.0 %
ISO 527
Flexural Modulus 1.25 GPa
181 ksi
ISO 178
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
ISO 306