Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 75000 - 150000 cP | 75000 - 150000 cP | Base, RFV #7 at 20 rpm |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Brookfield Viscosity | 75000 - 175000 cP | 75000 - 175000 cP | RVF, #7 spindle @ 4 rpm |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |
|||
Brookfield Viscosity | 75000 - 150000 cP | 75000 - 150000 cP | Base, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Brookfield Viscosity | 75000 - 150000 cP | 75000 - 150000 cP | Base, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |