Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 700000 - 900000 cP | 700000 - 900000 cP | Base, RVF #7 sp @ 2 rpm |
3M AC-215 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-215 Class B are two-part, polysulfide access door sealants for faying surfaces where easy separation of jointed surfaces is required. They are a highly thixotropic reddish pa.. |
|||
Brookfield Viscosity | 700000 - 900000 cP | 700000 - 900000 cP | Base, RVF #7 sp @ 2 rpm |
3M AC-215 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-215 Class B are two-part, polysulfide access door sealants for faying surfaces where easy separation of jointed surfaces is required. They are a highly thixotropic reddish pa.. |
|||
Brookfield Viscosity | 350000 - 900000 cP | 350000 - 900000 cP | RVT 'T'-spindle D@ 2.5 rpm |
3M Scotch-Weld™ PS67 Pipe Sealant Anaerobic Adhesives 3M™ Scotch-Weld™ Pipe Sealant Anaerobic Adhesives are one-component anaerobic sealants that cure and seal hydraulic and pneumatic pipes and fittings to withstand high temperatures and pressures. P.. |
|||
Brookfield Viscosity | 550000 - 900000 cP | 550000 - 900000 cP | Accelerator, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |