3M Scotch-Weld™ PS67 Pipe Sealant Anaerobic Adhesives

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ PS67 Pipe Sealant Anaerobic Adhesives.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Pipe Sealant Anaerobic Adhesives are one-component anaerobic sealants that cure and seal hydraulic and pneumatic pipes and fittings to withstand high temperatures and pressures. PS67 is a fast cure, low breakaway torque strength, high temperature past pipe sealant for metal connections in applications such as pressure vessels, air compressors, hydraulic, and pneumatic systems. It works on inactive surfaces (such as stainless steel) and provides and almost instant low pressure seal. A high pressure seal results when the bond is fully cured.Information provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity 350000 - 900000 cP
350000 - 900000 cP
RVT 'T'-spindle D@ 2.5 rpm
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance White Paste