Polymer Property : Brookfield Viscosity = 900000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 700000 - 900000 cP
700000 - 900000 cP
Base, RVF #7 sp @ 2 rpm
3M AC-215 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-215 Class B are two-part, polysulfide access door sealants for faying surfaces where easy separation of jointed surfaces is required. They are a highly thixotropic reddish pa..
Brookfield Viscosity 700000 - 900000 cP
700000 - 900000 cP
Base, RVF #7 sp @ 2 rpm
3M AC-215 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-215 Class B are two-part, polysulfide access door sealants for faying surfaces where easy separation of jointed surfaces is required. They are a highly thixotropic reddish pa..
Brookfield Viscosity 350000 - 900000 cP
350000 - 900000 cP
RVT 'T'-spindle D@ 2.5 rpm
3M Scotch-Weld™ PS67 Pipe Sealant Anaerobic Adhesives
3M™ Scotch-Weld™ Pipe Sealant Anaerobic Adhesives are one-component anaerobic sealants that cure and seal hydraulic and pneumatic pipes and fittings to withstand high temperatures and pressures. P..
Brookfield Viscosity 550000 - 900000 cP
550000 - 900000 cP
Accelerator, RVF #7 spindle, 20 rpm
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..