Physical Properties Metric English Comments
Viscosity Test 0.850 - 170 cm³/g

@Temperature 30.0 - 30.0 °C
0.850 - 170 cm³/g

@Temperature 86.0 - 86.0 °F
Average value: 46.5 cm³/g Grade Count:7
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Viscosity Test 150 - 170 cm³/g
150 - 170 cm³/g
Average value: 157 cm³/g Grade Count:3
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..