Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : ESCR 100% Igepal® = 4.0 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
ESCR 100% Igepal® 4.0 hour

@Thickness 3.80 mm,
Temperature 50.0 °C
4.0 hour

@Thickness 0.150 in,
Temperature 122 °F
non slit; ASTM D1693
Lotte Chemical Titan TITANEX® LI5011 Linear low density polyethylene resin  (discontinued **)
LI5011 is a pelleted high flow linear low density polyethylene. The higher melting point of the resin allows for higher end-use temperatures.Applications: House-wares, toys, lids, containers.Advan..
ESCR 100% Igepal® <= 4.0 hour

@Temperature 50.0 °C
<= 4.0 hour

@Temperature 122 °F
h/F50; Compression molded 2mm notched-plaques; ASTM D1693
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene
Description: SHA7260 is a high-density polyethylene, developed for the injection molding, easy to process and with high productivity. This resin has a good melt flow with high rigidity and hardness...
ESCR 100% Igepal® <= 4.0 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
<= 4.0 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Braskem HC7260LS-L HDPE Injection Molding Polyethylene
HC7260LS-L is a high-density polyethylene developed for injection molding. It has high hardness and stiffness and low warpage. This resin also has additives against ultraviolet radiation action. Its..
ESCR 100% Igepal® <= 4.0 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
<= 4.0 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Braskem HA7260 HDPE Injection Molding Polyethylene
HA7260 is a high-density polyethylene that was developed for injection molding. It is easy to process and has high productivity, high rigidity and hardness, and a good melt flow. Its narrow molar ma..
ESCR 100% Igepal® <= 4.0 hour

@Temperature 50.0 °C
<= 4.0 hour

@Temperature 122 °F
h/F50; Compression molded 2mm notched-plaques; ASTM D1693
Braskem Green PE SHC7260 Injection Molding High Density Polyethylene
Description: SHC7260 is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. The minimum biobased content of ..