Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP FARADEX WX94736 PBT
LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0090 - 0.010 cm/cm

@Time 86400 sec
0.0090 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific)
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0090 - 0.010 cm/cm

@Time 86400 sec
0.0090 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific)
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP UAL22S PPA
LNP* LUBRICOMP* UAL22S is a compound based on Polyphthalamide resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant, Heat Stabilized.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP ZI001XXX PPE+PS (Asia Pacific)
LNP* Lubricomp* ZI001XXX is a compound based on PPE+PS Blend resin.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 - 4.60 mm
0.0080 - 0.010 in/in

@Thickness 0.126 - 0.181 in
SABIC Method
SABIC Innovative Plastics Valox® 457 PBT
6.5% GR PBT, UL94 V-0/5V.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 - 4.60 mm
0.0080 - 0.010 in/in

@Thickness 0.126 - 0.181 in
SABIC Method
SABIC Innovative Plastics Valox® 457 PBT (Asia Pacific)
6.5% GR PBT, UL94 V-0/5V.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® 745 PBT
30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 6.40 mm
0.0080 - 0.010 in/in

@Thickness 0.252 in
SABIC Method
SABIC Innovative Plastics Valox® DR48M PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 6.40 mm
0.0080 - 0.010 in/in

@Thickness 0.252 in
SABIC Method
SABIC Innovative Plastics Valox® PDR4910 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS
LNP* STAT-LOY* AF3009 is a compound based on ABS resin containing 10% Glass Fiber. Added features of this material include: Antistatic, Flame Retardant.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific)
LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT (Asia Pacific)
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT (Asia Pacific)
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® 745 PBT (Asia Pacific)
30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT (Asia Pacific)
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT (Asia Pacific)
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 6.40 mm
0.0080 - 0.010 in/in

@Thickness 0.252 in
SABIC Method
SABIC Innovative Plastics Valox® VC108 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 6.40 mm
0.0080 - 0.010 in/in

@Thickness 0.252 in
SABIC Method
SABIC Innovative Plastics Valox® VGF4715 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 6.40 mm
0.0080 - 0.010 in/in

@Thickness 0.252 in
SABIC Method
SABIC Innovative Plastics Valox® VSR4150 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.