Material Notes:
Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.80 - 2.30 g/cc
1.80 - 2.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 67 - 81
67 - 81
ASTM D2240
Tensile Strength >= 1.03 MPa
>= 150 psi
ASTM D412
Elongation at Break >= 50 %
>= 50 %
ASTM D412
Tear Strength >= 6.14 kN/m
>= 35.0 pli
ASTM D624
Compression Set <= 30 %

@Temperature 100 °C,
Time 252000 sec
<= 30 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395, Method B
Thermal Properties Metric English Comments
Thermal Conductivity 0.900 W/m-K

@Pressure 2.07 MPa
6.25 BTU-in/hr-ft²-°F

@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flex TR10
Electrical Properties Metric English Comments
Volume Resistivity <= 0.25 ohm-cm
<= 0.25 ohm-cm
without pressure-sensitive adhesive; CEPS-0002
Shielding Effectiveness >= 95 dB

@Frequency 1.00e+8 Hz
>= 95 dB

@Frequency 1.00e+8 Hz
E Field; Method 3, CHO-TM-TP09
>= 100 dB

@Frequency 1.00e+10 Hz
>= 100 dB

@Frequency 1.00e+10 Hz
Plane Wave; Method 3, CHO-TM-TP09
>= 110 dB

@Frequency 2.00e+9 Hz
>= 110 dB

@Frequency 2.00e+9 Hz
Plane Wave; Method 3, CHO-TM-TP09
Descriptive Properties Value Comments
Binder Fluorosilicone
Filler Ni/Al
Heat Aging <0.25 ohm-cm
CEPS-0002