Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 210 MPa | 30500 psi | |
Poco Graphite DFP-1C (Copper impregnated) Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Compressive Strength | 210 - 240 MPa | 30500 - 34800 psi | ISO 604 |
Perstorp Compounds Aminel FX Melamine Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp .. |
|||
Compressive Strength | 210 MPa | 30500 psi | |
SGL Carbon Group EK 2240 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 210 MPa | 30500 psi | |
SGL Carbon Group EK 2241 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 210 MPa | 30500 psi | |
SGL Carbon Group EK 3235 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 210 MPa | 30500 psi | ASTM D695 |
Sumitomo Bakelite North America E 8354-19189-2 Electrical Encapsulation Grade Epoxy Glass and mineral reinforced epoxy molding compound, formulated for the encapsulation of devices requiring high quality and thermal shock resistance.Information provided by Vyncolit, a Sumitomo Bak .. |
|||
Compressive Strength | 210 MPa | 30500 psi | ASTM D695 |
Sumitomo Bakelite North America EM 7400-2 Long Glass Fiber Reinforced Epoxy EM 7400-2 is a polyaramide fiber reinforced epoxy molding compound, which features abrasion resistance and light weight.Information provided by Sumitomo Bak North America, Inc. |
|||
Compressive Strength | 210 MPa | 30500 psi | ASTM D695 |
Sumitomo Bakelite North America Epiall® 1904B-1 Short Glass Fiber Reinforced Epoxy Epiall 1904B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided .. |
|||
Compressive Strength | 210 MPa | 30500 psi | |
SGL Carbon Group Ridurid® V 1640 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 210 MPa | 30500 psi | ASTM D695 |
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta.. |
|||
Compressive Strength | 210 MPa | 30500 psi | ASTM D695 |
Sumitomo Bakelite North America E 2748A Short Glass Fiber Reinforced Epoxy E 2748A is a glass reinforced epoxy molding compound, with good impact strength combined with soft flow for the encapsulation of devices requiring high quality and thermal shock resistance.Informati.. |
|||
Compressive Strength | 210 MPa | 30500 psi | ASTM D695 |
Sumitomo Bakelite North America XB-22 Fiberglass Reinforced Phenolic Novolac XB-22 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is formulated for low thermal condu.. |
|||
Compressive Strength | 210 MPa | 30500 psi | ISO 604 |
Chevron Phillips Xtel® XE5030BL Polyphenylene Sulfide Alloy Xtel® XE5030BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevr.. |
|||
Compressive Strength | 210 MPa @Temperature 23.0 °C |
30500 psi @Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Compressive Strength | 210 MPa | 30500 psi | ASTM D695 |
Sumitomo Bakelite North America FM 4005X4649 Fiberglass Reinforced Phenolic Novolac FM 4005X4649 a fiberglass reinforced two-step phenolic molding compound formulated to increase thermal conductivity, to provide static dissipation and good wear resistance to abrasive media.Informat.. |