Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SGL Carbon Group Ridurid® V 1640 High Performance Graphite Filled Plastic

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer SGL Carbon Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SGL Carbon Group Ridurid® V 1640 High Performance Graphite Filled Plastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: Seals, compressors, pumps, bearingsInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
Open Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
Ball Size/Load - 5/100
Modulus of Elasticity 13.8 GPa
2000 ksi
Flexural Strength 93.1 MPa
13500 psi
Compressive Strength 210 MPa
30500 psi
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 20.0 °C
8.90 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 3.46 W/m-K
24.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C
350 °F
In oxygen
Maximum Service Temperature, Inert 204 °C
399 °F
Reducing Atm.
Users viewing this material also viewed the following: