Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 350 MPa | 50800 psi | ISO 604 |
Sumitomo Bakelite North America RX® 613 Fiberglass Reinforced Phenolic RX® 613 is a fiberglass reinforced phenolic molding compound with good dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bakelite North America, In.. |
|||
Compressive Strength | 350 MPa | 50800 psi | ASTM D695 |
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite HexMC® is a high performance carbon molding composite, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume content enable components to be molded for a wide.. |
|||
Compressive Strength | 350 MPa @Treatment Temp. 20.0 °C, Time 3600 sec |
50800 psi @Treatment Temp. 68.0 °F, Time 1.00 hour |
ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope.. |
|||
Compressive Strength | >= 350 MPa | >= 50800 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity.Information.. |
|||
Compressive Strength | >= 350 MPa | >= 50800 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame ret.. |
|||
Compressive Strength | >= 350 MPa | >= 50800 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Compressive Strength | >= 350 MPa | >= 50800 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Compressive Strength | >= 350 MPa | >= 50800 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Compressive Strength | >= 350 MPa | >= 50800 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe EP GM 202 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Compressive Strength | >= 350 MPa | >= 50800 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe EP GM 201 Glass Mat Reinforced Epoxy Resin - Sheet Used in mechanical and electrical applications. Extremely high mechanical strength at moderate temperature. Very good electrical properties under high humidity.Information provided by Hippe. |
|||
Compressive Strength | >= 350 MPa | >= 50800 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Compressive Strength | >= 350 MPa | >= 50800 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe EP GM 204 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Compressive Strength | 350 MPa @Temperature 200 °C |
50800 psi @Temperature 392 °F |
EN ISO 604 |
Brandenburger BRA_GLA 3 Thermal Insulation Board A material with high quality glass fibre fabric and roving layers in conjunction with heat resistant EP matrix, which provides a thermal protection with excellent compressive and flexural strength, .. |