Polymer Property : Compressive Strength = 50800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 350 MPa
50800 psi
ISO 604
Sumitomo Bakelite North America RX® 613 Fiberglass Reinforced Phenolic
RX® 613 is a fiberglass reinforced phenolic molding compound with good dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bakelite North America, In..
Compressive Strength 350 MPa
50800 psi
ASTM D695
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite
HexMC® is a high performance carbon molding composite, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume content enable components to be molded for a wide..
Compressive Strength 350 MPa

@Treatment Temp. 20.0 °C,
Time 3600 sec
50800 psi

@Treatment Temp. 68.0 °F,
Time 1.00 hour
ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets
Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope..
Compressive Strength >= 350 MPa
>= 50800 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity.Information..
Compressive Strength >= 350 MPa
>= 50800 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame ret..
Compressive Strength >= 350 MPa
>= 50800 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Compressive Strength >= 350 MPa
>= 50800 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Compressive Strength >= 350 MPa
>= 50800 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Compressive Strength >= 350 MPa
>= 50800 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe EP GM 202 Glass Mat Reinforced Epoxy Resin - Sheet
Compressive Strength >= 350 MPa
>= 50800 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe EP GM 201 Glass Mat Reinforced Epoxy Resin - Sheet
Used in mechanical and electrical applications. Extremely high mechanical strength at moderate temperature. Very good electrical properties under high humidity.Information provided by Hippe.
Compressive Strength >= 350 MPa
>= 50800 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet
Compressive Strength >= 350 MPa
>= 50800 psi
Perpendicular to laminations; IEC 1212-2 5.3
Hippe EP GM 204 Glass Mat Reinforced Epoxy Resin - Sheet
Compressive Strength 350 MPa

@Temperature 200 °C
50800 psi

@Temperature 392 °F
EN ISO 604
Brandenburger BRA_GLA 3 Thermal Insulation Board
A material with high quality glass fibre fabric and roving layers in conjunction with heat resistant EP matrix, which provides a thermal protection with excellent compressive and flexural strength, ..