Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D2837 |
Polymer Industries Densetec HDPE Pipe Grade The material displays improved performance characteristics in a variety of piping applications. In addition the material is UV stabilized and ideal for use in demanding outdoor applications. It reta.. |
|||
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D2837 |
Chevron Phillips Marlex® HHM TR-480X HDPE Pipe and Corrugated Extrusion Resin
(discontinued **) Characteristics: Good long-term hoop strength performanceVery high melt strengthOutstanding low temperature toughnessApplications: Municipal, industrial, and mining pipeOil and gas gathering pipeInf.. |
|||
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D2837 |
Chevron Phillips Marlex® HHM TR-480XC HDPE Pipe and Corrugated Extrusion Resin
(discontinued **) Characteristics: Good long-term hoop strength performanceVery high melt strength>Outstanding low temperature toughnessApplications: Municipal, industrial, and mining pipeOil and gas gathering pipeIn.. |
|||
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D-2837 |
Chevron Phillips Marlex® H516 Polyethylene; HDPE
(discontinued **) High density polyethylene compound. This high performance PE 100 HDPE compound is tailored for the demanding requirements of pressure pipe applications that require: Excellent long-term hoop stren.. |
|||
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D 2837 |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D 2837 |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Hydrostatic Design Basis | 11.0 MPa | 1600 psi | ASTM D2837 |
LyondellBasell Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade Alathon L4904 is a bimodal, high molecular weight, high density polyethylene resin with excellent processability characteristics that meet the high performance requirements of demanding pressure pip.. |
|||
Hydrostatic Design Basis | 11.0 MPa | 1600 psi | ASTM D2837 |
LyondellBasell Alathon® L5008HP High Density Polyethylene, Pressure Pipe Extrusion Grade ALATHON L5008HP is a bimodal, high molecular weight, high density polyethylene resin with excellent processability designed to meet the high performance requirements of pressure pipe applications in.. |
|||
Hydrostatic Design Basis | 11.0 MPa | 1600 psi | ASTM D2837 |
Ineos K44-15-122 HDPE K44-15-122 is a natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF S.. |
|||
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D2837 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. .. |
|||
Hydrostatic Design Basis | 11.0 MPa | 1600 psi | ASTM D2837 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. I.. |
|||
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D2837 |
Ineos TUB 121 HDPE TUB 121 (aka ELTEX® TUB 121, ELTEX® TUB 121 N2025, and ELTEX® TUB 121 N3000) is a black high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, ind.. |
|||
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D2837 |
Ineos TUB 121N HDPE TUB121N is a natural high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, industrial, and mining pipe. When blended with an approved black concentrate, t.. |
|||
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D2837 |
Ineos TUB 121NTW HDPE TUB121 NTW is a natural high density bimodal polyethylene copolymer designed for extrusion of large diameter, thick wall piping for potable water, industrial and mining applications. When blended wi.. |
|||
Hydrostatic Design Basis | 11.0 MPa | 1600 psi | ASTM D2837 |
Ineos K44-06-122 HDPE HDPE K44-06-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as .. |
|||
Hydrostatic Design Basis | 11.0 MPa | 1600 psi | ASTM D2837 |
Ineos K44-08-122 HDPE K44-08-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as havin.. |
|||
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D 2837 |
Total HP 401N Natural HDPE, pipe Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by T.. |
|||
Hydrostatic Design Basis | 11.0 MPa | 1600 psi | 100,000 hrs.; ASTM D2837 |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |
|||
Hydrostatic Design Basis | 11.0 MPa @Temperature 23.0 °C |
1600 psi @Temperature 73.4 °F |
ASTM D 2837 |
Total XT10 N Natural HDPE, pipe Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe.. |