Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412 |
Northstar Polymers MPP-A90A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412 |
Techmer ES Luriblend® TPU 40D GL10 Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant(10%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412-92 |
Saint-Gobain Tygothane® C-544-AI.B. Precision Polyurethane Pressure Tubing Formulation Description: Tygothane® C-544-A I.B.: More flexible than many other reinforced urethane tubings, Tygothane® Pressure Tubing can be used in some of the most physically demanding applications,.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | |
Elastomer Engineering E850-85A Polyurethane A very tough and cut-resistant polyether-based formulation with good dynamic properties that bonds well to all metals. Information provided by Elastomer Engineering Inc (EEI) |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412 |
Lubrizol Estane® ALR PC85A Thermoplastic Polyurethane Type: Estane® ALR PC85A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00552 GPa | 0.801 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, No Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D638 |
Colorite Polymers 8087 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D638 |
Colorite Polymers 93-635A General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | |
Colorite Polymers Self Frosting™ 6811SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D-638 |
Axiall 8702 Moldings & Extrusions Flexible PVC General purpose, elastomeric vinyl compound well suited for co-extrusion with rigid PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412 |
Advanced Polymer Alloys DURACRYN 8080 NC Thermoplastic Rubber Information provided by Advanced Polymer Alloys |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D-638 |
Axiall 1802 Moldings & Extrusions Flexible PVC Flexible PVC compound designed for food and beverage tubing applications per CFR21 and NSF61. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axia.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D-638 |
Axiall 801-90B Moldings & Extrusions Flexible PVC Automotive harness tape.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D-638 |
Axiall 8745 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D-638 |
Axiall 8770 Moldings & Extrusions Flexible PVC General purpose extrusion compound for weatherstrips, tubings and gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D-638 |
Axiall 8808 Moldings & Extrusions Flexible PVC 105°C rated flexible polyvinyl chloride compound formulated for UL94 V-2 in all colors. The compound is formulated for sunlight resistance.Information provided by Georgia GulfGeorgia Gulf became A.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FE 5610 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5610 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D638 |
Colorite Polymers 6800-UV General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | |
Colorite Polymers 6811 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | |
Colorite Polymers 6812 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D638 |
Colorite Polymers 7075 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00552 GPa | 0.801 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, No Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D-638 |
Axiall 8681 Moldings & Extrusions Flexible PVC General purpose, elastomeric vinyl compound well suited for co-extrusion with rigid PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412-98 |
Saint-Gobain Tygothane® C-210-A Precision Polyurethane Tubing Formulation Description: Tygothane® C-210-A: Our rigidly controlled manufacturing process makes Tygothane® Precision Polyurethane Tubing the flexible polyurethane tubing that has consistently tight toleranc.. |