Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | >= 0.00300 GPa | >= 0.435 ksi | DIN 53504 |
NEXA® PFX9010 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Trefsin® 3201-65 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ISO/R527 |
Polykemi AB POLYelast TPE ZSB60650 Thermoplastic Elastomer, SEBS/SBS-based, Mineral Reinforced Information provided by Polykemi AB |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 5.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® CA116-203 TPU-Polyester Introduction: IROGRAN CA116-203 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-203 is part of the HUNTSMAN film and shee.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® CA116-205 TPU-Polyester Introduction: IROGRAN CA116-205 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-205 is part of the HUNTSMAN film and shee.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8170 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 5.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D412 |
Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: High MVTRAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 402701S SBS Based Material, 70A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 500700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 502700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 502750S SEBS Based Material, Unfilled Qualities, 75A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 600650S SEBS Based Material, Filled Qualities, 65A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 600700S SEBS Based Material, Filled Qualities, 70A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 602650S SEBS Based Material, Filled Qualities, 65A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 602700S SEBS Based Material, Filled Qualities, 70A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 660650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 660700S SEBS Based Material, Semi-Filled Qualities, 70A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 662700S SEBS Based Material, Semi-Filled Qualities, 70A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Dryflex® 662750S SEBS Based Material, Semi-Filled Qualities, 75A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D638 |
ELASTO UK Mediprene™ 500750M TPE, Medical Applications, 75A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4520 General Purpose Compound FormulationNordel® IP 4520 |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ASTM D412 |
Advanced Polymer Alloys Alcryn® 2170 BK Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | ISO 37 |
AlphaGary Evoprene™ G 975 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
100% Modulus | 0.00300 GPa | 0.435 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Trefsin® 3101-65 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |