Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.00 - 2.30 GPa | 290 - 334 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_7220 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide .. |
|||
Modulus of Elasticity | 1.70 - 2.30 GPa | 247 - 334 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8505Gray20 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Modulus of Elasticity | 1.70 - 2.30 GPa | 247 - 334 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8505Gray25 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Modulus of Elasticity | 1.70 - 2.30 GPa | 247 - 334 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Modulus of Elasticity | 1.70 - 2.30 GPa | 247 - 334 ksi | ASTM D638-04 |
Proto3000 Objet Digital Materials™ DM_8505Gray40 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Modulus of Elasticity | 0.140 - 2.30 GPa @Temperature -40.0 - 150 °C |
20.3 - 334 ksi @Temperature -40.0 - 302 °F |
Average value: 1.32 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Modulus of Elasticity | 1.24 - 2.30 GPa | 180 - 334 ksi | Average value: 1.65 GPa Grade Count:8 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Modulus of Elasticity | 1.20 - 2.30 GPa @Temperature 60.0 - 90.0 °C |
174 - 334 ksi @Temperature 140 - 194 °F |
Average value: 1.67 GPa Grade Count:3 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |