Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tisan TISREN® Flame Retardant (V0) Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer Tisan Engineering Plastics
Trade Name TISREN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tisan TISREN® Flame Retardant (V0) Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TISREN has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimensional stabilityInsulationLow weightHigh toughnessLow moisture absorptionHigh chemical resistance It has excellent chemical resistance to weak acids, weak alkalis, and strong alkalis. It has good resistance against strong acids. It has weak chemical resistance against organic solvents, alcohols, hydrocarbons, and engine fuels.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 527-2
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527-2
Elongation at Break 3.0 %
3.0 %
ISO 527-2
Elongation at Yield 3.5 %
3.5 %
ISO 527-2
Modulus of Elasticity 2.20 GPa
319 ksi
ISO 527-2
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Vicat Softening Point 104 °C
219 °F
ISO 306
Heat Distortion Temperature 94.0 °C
201 °F
ISO 75-2
Flammability, UL94 V-0
V-0
Glow Wire Test 960 °C
1760 °F
60695-2-10
Electrical Properties Metric English Comments
Comparative Tracking Index 250 V
250 V
TS EN 60112
Processing Properties Metric English Comments
Feed Temperature 60.0 °C
140 °F
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Aft-1. Region Temperature
Middle Barrel Temperature 190 - 210 °C
374 - 410 °F
Mid-2. Region Temperature
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Pre-3. Region Temperature
Nozzle Temperature 200 °C
392 °F
Melt Temperature 160 - 180 °C
320 - 356 °F
Drying Temperature 80.0 °C
176 °F
Predrying Temperature
Dry Time 2 - 3 hour
2 - 3 hour
Predrying Time
Moisture Content 0.30 %
0.30 %
ISO 62
Descriptive Properties Value Comments
Block Temperature 45°C