Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.80 - 6.20 GPa | 406 - 899 ksi | Average value: 4.54 GPa Grade Count:54 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Modulus of Elasticity | 1.72 - 6.20 GPa | 250 - 899 ksi | Average value: 3.26 GPa Grade Count:20 |
Overview of materials for Polypropylene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app.. |