Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.80 GPa | 406 ksi | ASTM D638 |
Plaskolite Optix® CA-41 General Purpose Acrylic Resin Injection Molding Grade Pellets only. Lowest Heat Resistance and maximum flow. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | dry |
Murtfeldt Murytal® C Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | 50% RH |
Murtfeldt Murytal® C Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Modulus of Elasticity | 2.80 - 6.20 GPa | 406 - 899 ksi | Average value: 4.54 GPa Grade Count:54 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Modulus of Elasticity | 2.80 - 13.8 GPa | 406 - 2000 ksi | Average value: 7.28 GPa Grade Count:22 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Modulus of Elasticity | 2.80 - 3.70 GPa | 406 - 537 ksi | Average value: 3.20 GPa Grade Count:5 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | |
Lehmann & Voss LUVOCOM® 50-8479/BL Polycarbonate, unreinforced Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Isotropic shrinkage characteristics.Reduced moment of inertia .. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | |
Lehmann & Voss LUVOCOM® 6-7834 Polyamide 12, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion, for dimensional stable precision parts.Isotropic sh.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | ISO 527 |
GEHR Plastics ECOGEHR® PLA-LF Polylactic Acid PLA-L is a blend of polylactide, lignin, lingo-cellulosic, natural fatty acids, waxes and wood fibers. This material possesses good mechanical properties similar to ABS. This bioplastic has an opera.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | ISO 527-2 |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | Plain Cast Resin; ASTM D638 |
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 35LH247 OPP Film Product Description: A super white opaque, caviated BOPP film for Pressure Sensitive (PSA) labeling applications where superior optics are desired. LH247 also shows excellent performance on reel-fed.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 40LH247 OPP Film Product Description: A super white opaque, caviated BOPP film for Pressure Sensitive (PSA) labeling applications where superior optics are desired. LH247 also shows good performances on reel-fed wra.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 40MH247 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film. This opaque and stiff film is ideal for mono material requirements and it has been especial.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 42AH748 OPP Film Product Description: A high barrier, high speed, super white opaque, modified higher density biaxially oriented polypropylene film, coated one side high barrier PVdC, one side very low temperature s.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 42MH647 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Ava.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 42MH648 OPP Film Product Description: A high speed super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated one side acrylic, one side very low temperature seal (VLTS) coati.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 50MH247 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film. This opaque and stiff film is ideal for mono material requirements and it has been especial.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 52MH647 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Ava.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 52MH648 OPP Film Product Description: A high speed super white opaque, modified higher density, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 52MHR647 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented PP film, humidity resistant acrylic coated two sides. This film is designed to wrap products with a high moistu.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | ISO 527-2 |
BASF Ultraform® W2320 003 PRO POM Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | ISO 527-2 |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | ISO 527 |
BASF Ultramid® B3L PA6 (Dry) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | ISO 178 |
Addiplast Addinyl A2 Nylon 66 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | ISO 178 |
Addiplast Addinyl C2 Nylon 66/6 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | ISO 527-1/-2 |
BASF Ultramid® B3L BK00464 PA6 (Dry) Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall .. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | TD; ExxonMobil Method |
ExxonMobil Oppalyte™ 35HM247 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film. This opaque and stiff film is ideal for mono material requirements and it has been especial.. |
|||
Modulus of Elasticity | 2.80 - 3.30 GPa | 406 - 479 ksi | Average value: 3.17 GPa Grade Count:4 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Modulus of Elasticity | 2.80 GPa | 406 ksi | ISO 178 |
Addiplast Addinyl B2 Nylon 6 Unreinforced, medium viscosityInformation provided by Addiplast. |