Material Notes:
TRA-BOND 813J01 is a silicone adhesive system formulated to provide excellent thermal conductivity. This unique product bonds well to difficult substrates. Typical applications include encapsulation of heat generating devices such as transformers, thermistors or power sources and pour-in-place heat sinks. TRA-BOND 813J01 exhibits very low stress upon cure thus preventing component cracking and other stress related problems. It can be room temperature cured in thick or thin sections. This non-corrosive potting material will not revert when exposed to high temperatures. TRA-BOND 813J01 has a 6 month shelf life when stored at 25°C. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 2.10 g/cc
2.10 g/cc
Mixed
Viscosity 40000 cP
40000 cP
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Adhesive Bond Strength 3.45 MPa
500 psi
Lap shear, alum to alum
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 20.0 °C
111 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Glass Transition Temp, Tg -120 °C
-184 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Processing Properties Metric English Comments
Cure Time 20.0 min

@Temperature 150 °C
0.333 hour

@Temperature 302 °F
60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
2880 - 10100 min

@Temperature 25.0 °C
48.0 - 168 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Red
Mix Ratio, parts by weight 100/100
Resin/Hardener
Working Life minutes 100
100 grams