Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00980 GPa | 1.42 ksi | DIN 53504 |
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
300% Modulus | 0.00980 GPa | 1.42 ksi | ASTM D412 |
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |