Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00980 GPa | 1.42 ksi | DIN 53504 |
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
300% Modulus | 0.00981 GPa @Temperature 145 °C, Time 2100 sec |
1.42 ksi @Temperature 293 °F, Time 0.583 hour |
cured; ASTM D412 |
LG Chemical BR 1280 Polybutadiene Polymer BR 1280 is high cis- 1,4 polybutadiene polymer produced by a solution polymerization process polymerization process employing a stereospecific catalyst to control microstructure, molecular weight an.. |
|||
300% Modulus | 0.00981 GPa | 1.42 ksi | Cured |
KKPC Kumho KHS 58 High Styrene Resin Masterbatch (HSR) High Styrene Resin Masterbatch (HSR)Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improve.. |
|||
300% Modulus | 0.00981 GPa @Temperature 145 °C, Time 2100 sec |
1.42 ksi @Temperature 293 °F, Time 0.583 hour |
ASTM D412 |
LG Chemical SBR 1783 High Acrylonitrile Polymer Description: SBR 1783 is an oil extended cold polymerization SBR with 37.5 parts of aromatic oil and styrene-butadiene copolymer of 23.5% bound styrene. Raw materials for this product are carefully.. |
|||
300% Modulus | 0.00981 GPa | 1.42 ksi | |
Taiwan Sheen Soon Sheenthane® A8556K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.00981 GPa | 1.42 ksi | |
Taiwan Sheen Soon Sheenthane® A8820N Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.00981 GPa | 1.42 ksi | |
Taiwan Sheen Soon Sheenthane® A9070A Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.00981 GPa | 1.42 ksi | |
Taiwan Sheen Soon Sheenthane® A9080 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.00980 GPa | 1.42 ksi | ASTM D412 |
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |