Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP EX03647H PEI LNP LUBRICOMP* EX03647H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp KFL36XXC Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL36 is an Acetal containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing proprietary fillers. Added features of this material include: Easy Molding, High Temperature Bearing Grade, Wear.. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp OFG26XXP PPS - Linear LNP* Lubricomp* OFG26XXP is a compound based on Linear PPS containing Glass Fiber and Graphite Powder. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for.. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 LNP* LUBRICOMP* RFL36XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP RFL46ES PA 66 LNP* LUBRICOMP* RFL46ES is a compound based on Nylon 6/6 containing 30% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized, Easy Molding. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP UX95672 PPA LNP LUBRICOMP* UX95672 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34 PBT LNP LUBRICOMP* WFL34 is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66 LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS (Asia Pacific) LNP* STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This da.. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON AE006 ABS LNP* STAT-KON* AE006 is a compound based on ABS containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS LNP* STAT-KON* AX02747 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific) LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon OEL36A PPS LNP* Stat-Kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This .. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON OEP32 PPS - Linear (Asia Pacific) LNP* STAT-KON* OEP32 is a compound based on PPS - Linear resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP AF004XXY ABS LNP* Thermocomp* AF004XXY is a compound based on ABS containing 20% glass fiber. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP JF006LZZ PES LNP THERMOCOMP* JF006LZZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Extrusion Grade, Low Extractable. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific) LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP PF006 PA 6 LNP THERMOCOMP* PF006 is a compound based on Nylon 6 resin containing 30% Glass Fiber. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66 LNP* THERMOCOMP* RC004SXS is a compound based on Nylon 66 containing 20% Carbon Fiber. Added feature of this grade includes: Heat Stabilized, Electrically Conductive. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon DX96690 PC LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America.. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 LNP* STAT-KON* REF42 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP MF742XXH PP LNP* THERMOCOMP* MF742XXH is a compound based on Polypropylene resin containing Glass Fiber and proprietary antimicrobial additives. This product is best suited for touch surfaces in healthcare app.. |
|||
Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl PX0346 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp MF0069S PP LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi.. |