Mechanical Properties Metric English Comments
Impact Test 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 43.0 J
31.7 ft-lb
Instrumented Impact, Total Energy; 2.5 mm thick, 7.6 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
Covestro Bayblend® 2773 Polycarbonate + ABS Blend, Automotive  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Impact Test 43.0 J
31.7 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRILOY D2000P PC
LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing, Wear Resistant.
Impact Test 43.0 J
31.7 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRILOY D2000P PC (Asia Pacific)
LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing.
Impact Test 43.0 J
31.7 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP DX09402 PC
LNP* THERMOCOMP* DX09402 is a compound based on Polycarbonate containing Proprietary Filler(s).
Impact Test 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 2642 ABS, Impact Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 342EZ ABS, Medium Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 348 ABS, Low Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 341 ABS, Low Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 43.0 J

@Temperature 23.0 °C
31.7 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 357HP ABS, High Heat
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 43.0 J

@Thickness 3.20 mm
31.7 ft-lb

@Thickness 0.126 in
Instrumented Total Impact; 3.2 mm thick, 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763
Covestro Bayblend® T 65 Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,..